Image of New Large Scale Condensate Receiver Tank. Courtesy of Charles Ross & Son Co.
CHARLES ROSS & SON CO.: Receiver Tank
The new 9,400-gallon condensate receiver tank from Ross Engineering is designed and built according to ASME standards for up to five psi at 200 ⁰F. The tank is constructed from 304 stainless steel and includes multiple nozzles for venting, instrumentation, and discharge, as well as a 24-inch API manway.
Ross Engineering custom fabricates tanks, pressure vessels, and reactors up to 100,000 gallons or larger that are used throughout the process industries for various manufacturing and storage functions. It also offers hydrotesting, passivation, ASME code stamp, ladders, jacketing, insulation, agitators, and other customizations.
To learn more, visit www.mixers.com.