Image of AGC Chemicals' Fluoroelastomers

Fluoroelastomers. Courtesy of AFLAS.

AGC CHEMICALS: Fluoroelastomers

September 8, 2023

AGC Chemicals Americas Inc., has added two new grades to its line of perfluoroelastomers.  AFLAS® FFKM PM-5000 and FFKM PM-5500 perfluorinated elastomers can be used for semiconductor plasma process applications due to their high temperature durability beyond 300 °C and excellent resistance to O2 and NF3 plasma. They have a high molecular weight that enables greater hardness without using fillers, which can create unwanted particles.

The new nitrile-curable grades build on the high-performance properties of other AFLAS FFKMs. They provide excellent chemical resistance and electrical insulation. These qualities make them suitable for fabricating components that perform in aggressive and sensitive environments.

To learn more, visit www.agcchem.com.