I require an adhesive for sticking paper to tins.

I can only assume you mean applying labels to metal containers.

There are any number of adhesives and processes available to accomplish this. Basically, there are two types of labels that are commonly in use. One makes use of a pressure sensitive adhesive that is pre-applied to the label stock (usually in rolls), and the label is then applied to the individual container.

The other type of label is typically referred to as a "patch label," and as the name implies, is supplied pre-cut and stacked. It can be applied either by the pre-application of a pressure sensitive adhesive, or more commonly by using a water-based adhesive to apply the label to the container when required.

This latter process usually involves highly automated application equipment and typically is employed for very high-volume applications. For lower-volume applications, the more labor-intensive method of a pre-applied pressure sensitive label is often the most economical approach, despite the significantly higher cost of the label itself.

BOB SMITH & ROGER LOHMAN

Is there a certain type of epoxy or compound, especially a one-part compound, that will adhere two pieces of polished granite together permanently for outdoor exposure?

Epoxies are recommended for such applications. However, they would all require some type of mechanical abrading of the surface in order to obtain a good bond.

Secondly, these products are two-component. I know of no one-component adhesive that might be used in this application, and would appreciate any suggestions from our readers. There are one-component epoxies - even supplied as reactive films - but they require refrigeration in shipping and storage before use and are somewhat expensive. They are generally not used in the type of application you describe.

Other adhesive types that could possibly be used in your application may not be good for outdoor exposure. For instance, a one-component cyanoacrylate might be used to bond polished granite, but the exposure to outside moisture, as well as vibration, would not make it a good choice.

ROGER LOHMAN

The ChemQuest Group, Inc., Cincinnati, has announced a special promotional offer of 15% off all Internet purchases of its online market data available by clicking on the shopping cart at www.chemquest.com. The promotional offer is obtained by entering the promotional code, cqdata1, upon registration, and applies to the company's extensive U.S. coatings, and U.S. and European adhesives market databases. These databases are constantly updated as new information becomes available. The offer expires on Sept. 14, 2001.

"This offer provides an introduction to our newly redeveloped Web site and a first look at our current coatings and adhesives market data. We are confident it will provide value and bring users back for additional visits," said Dan Murad, president of The ChemQuest Group. "We recognize the need to provide instant access to our specialized market information with the speed of the Internet," he added.

According to Murad, the data represents market sizes, market trends, technology trends, raw material trends and the emergence of growth opportunities that have been monitored by ChemQuest since 1976.

If you need assistance, have concerns about an on-line credit card purchase, or would like more detailed information about any piece of market data, contact The ChemQuest Group at www.chemquest.com, or call 513-469-7555.

Links