Creative Materials: Electrically Conductive Adhesive
September 11, 2000
This company’s new product, 118-09, is a two-component, solvent-resistant, electrically conductive ink, coating and adhesive suitable for screen-printing printed circuit lines. The product features excellent adhesion to Kapton, Mylar, glass, polycarbonate and a variety of other substrates. Unlike conventional conductive materials, 118-09 is very resistant to methyl ethyl ketone. It is also very resistant to scratching and creasing.