Northwest Coatings has filed for a U.S. Patent on its new UV/EB-curable laminating adhesive technology.
Northwest Coatings Corp., Oak Creek, Wis., has filed for a U.S. Patent on its new UV/EB-curable laminating adhesive technology. This new technology has shown a very low potential for migration through polyolefin substrates and provides excellent bonds on a variety of paper, film and metalized substrates.
Northwest Coatings Corp., Oak Creek, Wis., has filed for a U.S. Patent on its new UV/EB-curable laminating adhesive technology. This new technology has shown a very low potential for migration through polyolefin substrates and provides excellent bonds on a variety of paper, film and metalized substrates.