Ultra-Low Formaldehyde Adhesive Base



Air Products Polymers' Airflex® 315 emulsion is manufactured without any formaldehyde-containing or formaldehyde-generating chemicals, offering formulators an adhesive base with ultra-low levels of formaldehyde. This vinyl acetate-ethylene copolymer has a Tg of 17 °C, and its broad formulating latitude features fast setting speed, good clean up, and high wet tack.