TRA-CON: Epoxy Adhesive

March 21, 2005
TRA-BOND 2126 is a black, medium-viscosity and thixotropic epoxy adhesive with a high glass transition temperature and a Shore D hardness of 90. It has a pot life of 30 minutes and can be cured in 24 hours at room temperature, or more quickly at 65 degrees C. It has good impact resistance, low shrinkage and is an electrical insulator. It is also effectively resistant to many organic and inorganic compounds due to its rigidity. Finally, TRA-BOND 2126 is a flawlessly opaque system, perfect for photographic, industrial and laboratory bonding and laminating applications.