www.adhesivesmag.com/articles/86128-henkel-uv-visible-light-curing-silicone
HENKEL: UV/Visible Light-Curing Silicone
July 18, 2005
Loctite Nuva-Sil products from Henkel Corp. offer superior weather, temperature and moisture resistance for a range of applications, including deep potting, encapsulation, environmental protection, and sealing. Translucent in appearance, the silicones will not degrade or yellow under long-term light exposure. All three next-generation silicones offer a built-in fluorescence detection system that allows automatic quality inspection. Loctite 5031 Nuva-Sil is a self-leveling liquid that flows easily under parts for potting, encapsulation and sealing applications. Loctite 5039 Nuva-Sil is a semi-leveling paste ideal for gasketing and sealing that forms excellent beads with minimal knit lines or seams. And Loctite 5033 Nuva-Sil is a thixotropic paste for gasketing, sealing and potting applications that require a full-bodied material.
For more information, visithttp://www.loctite.com, call (800) LOCTITE or e-mail marketing@loctite.com.