CREATIVE MATERIALS INC.: Conductive Silicone Adhesives
August 11, 2014
102-32D is a new conductive silicone adhesive that can offer enhanced features over the company’s standard 102-32, which is reportedly one of the company’s most versatile and widely used products. These features include improved working life and dispensing characteristics.
102-32D was designed for high throughput and automated dispensing processes, allowing for enhanced features such as no tailing or stringing and low bleeding. The adhesive can provide high conductivity (0.0001 Ω-cm), high elasticity, resistance to high temperatures and thermal cycling, low bleeding, low modulus, and low stress.
For more information, visit www.creativematerials.com.