DELO: High-Temperature Adhesives
High-temperature adhesives from this company reportedly provide a temperature stability of 3 N/mm² at 220°C, as well as 12 N/mm² at 150°C. The epoxy resin adhesives can provide this performance due to an increased glass-transition temperature, as well as an improved long-term temperature stability. In addition, the adhesives can hold 80% of their initial tensile strength after being stored at +220°C for 1,000 hours.
Used as construction adhesives, DELOMONOPOX HT281 and the impact-resistant DELOMONOPOX HT282 are suitable for bonding metals, as well as temperature-resistant plastic, ferrite, and ceramic. The adhesives have high strength and permanent resistance to harsh environmental influences.
For more information, visit www.delo-adhesives.com.