September 9, 2014
This company now offers 3M’s new Scotch-Weld low-odor acrylic adhesives. The adhesives DP8805NS and DP8810NS have reportedly been formulated to provide excellent structural bonding without odor. In addition, the adhesive range offers a faster cure rate, reaching structural strength in nine minutes—reportedly less than half of the time required for standard acrylic adhesives.
The adhesives can offer improved adhesion and impact resistance on plastics and metals, as well as excellent shear and feel performance.