This company’s International® protective coatings brand has launched Enviroline® 2405, an advanced hybrid epoxy lining system. The high-temperature, abrasion-AKZONOBEL: Epoxy Lining Systemresistant coating was reportedly designed to offer flexibility, durability and protection in a single coat.

Enviroline 2405 is formulated as an ultra-high-solids, low-volatile-organic-compound (VOC), two-component polycyclamine-cured epoxy for faster and easier installation in a variety of oil and gas, chemical, mining, and water and wastewater environments. Applied at ambient temperature, with either standard airless or plural component spray equipment, the coating can provide a rapid hard cure in six hours, with a return to service in about 48 hours.