www.adhesivesmag.com/articles/93537-flexcon-pressure-sensitive-films
NewProducts.jpg

FLEXCON: Pressure-Sensitive Films

December 30, 2014

This company has announced the newest in its DPM® series of pressure-sensitive films designed for durable product marking: DPM U 150 silver V-29 150 poly H-9. The film’s mirror-like finish reportedly offers a brilliant metal look that is ideal for high-end durable labels, die-cut labels and decorative decals. Its conformability allows it to conform to extremely tight mandrel surfaces and around sharp corners, making it useful for graphics applied to compound surfaces. In addition, it is outdoor durable for five years.

The 1.5-mil silver urethane film has a permanent pressure-sensitive acrylic adhesive and polyester release liner, and is designed for product identification and labeling applications for the durable goods and transportation industries. The print-receptive surface is compatible with thermal transfer, UV flexo and UV screen, and the adhesive bonds well to both low- and high-surface energy plastics, metal, paint, and powder-coated paint.

For more information, visit www.flexcon.com.