TROY CORP.: Wetting and Dispersing Additive

January 5, 2015

Troysperse™ ZWD1 is a new 100% active liquid pigment wetting and dispersing additive for aqueous coating and printing ink applications. The additive can be used for the preparation of aqueous color pigment concentrates using organic color pigments. It is reportedly formulated for excellent color development, fast dispersion time, high gloss, and high pigment loading, and is effective at low use levels. In addition, it reportedly contributes zero VOCs to finished products, allowing more latitude in the formulation of ‘green’ products.