FLEXCON: Silicone Adhesive
June 25, 2015
A new, removable silicone adhesive product is now available from this company. FLEXcon® SA1000 reportedly offers clean removability, performance at temperatures as high as 400°F, and excellent clarity, allowing it to be used for electronic applications.
The adhesive can be used to affix films to smooth surfaces and provides consistent, clean, quiet removability. It can be provided on various films, based on application need, to create individualized solutions. In some cases, the product can be re-applied or used more than one time.
For more information, visit www.flexcon.com.