ITW DYNATEC: Hot Melt Supply Unit

March 16, 2016

This company has reportedly introduced a newer and more versatile Dynamini™ hot-melt adhesive supply unit (ASU). The unit feature a four-hose configuration, allowing for greater operational capabilities and reportedly making it suited for larger-sized applications as well as higher-volume multi-point applications. Built for flexibility, it can be configured with nickel or platinum (PT100) temperature sensors, and is designed to integrate with other industry standard components. It also features the company’s Melt-on-Demand™ technology.

Available in a four-hose or two-hose configuration, the unit can provide accurate, proportionate temperature control for hoppers, hoses, and applicators. Sequential start-up delays may be programmed for turn-on of the hoses and heads. The temperature control reportedly can interlock the parent machine so that production automatically begins when adhesive has reached the programmed application temperature.

For more information, visit www.itwdynatec.com