www.adhesivesmag.com/articles/94874-techsil-acrylate-adhesive

TECHSIL: Acrylate Adhesive
September 6, 2016
This company has introduced a newly developed light-curing acrylate adhesive from Panacol. Vitralit® 7311 is specially formulated for bonding plastics, metals, and glass and is available in three different viscosities: low viscosity, medium flow, and a non-flowing gel.
Vitralit reportedly cures in seconds with ultraviolet or visible light. For excellent curing results, high-intensity LEDs at 405 nm wavelength are recommended. This wavelength also permits the bonding of materials like polycarbonate, which block UV rays.
For more information, visit www.techsil.co.uk.