Reverdia Announces Biosuccinium Collaboration

Reverdia recently announced it has signed a strategic partnership with Hangzhou Xinfu.

November 22, 2016

Reverdia recently announced it has signed a strategic partnership with Hangzhou Xinfu Science & Technology Co. Ltd. (Xinfu). The partnership reportedly represents a collaboration to adopt Biosuccinium® in biobased polymers and co-polymers for the packaging industry, as well as a long-term supply agreement.

Xinfu is reportedly a global pioneer in fully biodegradable resins and films. It will exclusively use Biosuccinium for producing biobased polymers, derivatives, and new biomaterials for packaging applications such as compostable, single-use bags.

“These new materials will target the biodegradable packaging market,” said Marcel Lubben, president of Reverdia. “We’re excited to work with an industry pioneer like Xinfu on biobased solutions and this agreement is yet another example of Reverdia’s global leadership in value chain innovation.”

For more information, visit www.reverdia.com.