ORION ENGINEERED CARBONS: Brochure
A newly revised brochure from this company explores the range and function of high-performance specialty carbon blacks for semiconductive compounds used in high-voltage (HV) cables and extruded tape. The four-page color brochure (TI-1387) reportedly describes the role of specialty carbon blacks as primary components of HV cables and extruded tape. It reviews the importance of surface smoothness, cleanliness, conductivity, low-sulfur impurities, and high melt flow rate to the development of high-performance specialty carbon black, and it charts the performance and technical attributes of five Orion high-performance grades. These products can support HV cables low energy loss during long-distance transmission.
For more information, visit www.orioncarbons.com.