Hand-on-Keyboard

Ashland Receives Patent

The technology tandem reportedly creates a coating for flexible packaging that is water and scuff resistant.

June 26, 2017

Ashland recently announced it has received U.S. patent 9,539,795 for its PureKoteā„¢ 23589 dispersion and PureKoteā„¢ 21412A crosslinking agent coating system. The technology tandem reportedly creates a coating for flexible packaging that is water and scuff resistant, and has a soft-touch feel and matte finish. The coating system can reportedly be used safely in food packaging applications regulated by the U.S. Food and Drug Administration, including paper and plastic bags, pouches, lidding films, foil bags, and sachets.  

For more information, visit www.ashland.com.