MACTAC: Double-Coated Tape

July 5, 2018

This company recently announced the addition of permanent/removable double-coated tape to its MACbondâ„¢ double-coated tapes product line.  IB5121-72 features 1.2-mil XT high-performance rubber adhesive on the unwind side of a 0.5-mil PET carrier and a 1-mil low-tack removable acrylic adhesive on the liner side. The dual-performance adhesive is reportedly protected by a two-side silicone-coated 72# bleached poly-coated, dimensionally stable liner.