LORD: Polyurethane Adhesive

August 21, 2018

This company recently announced the launch of LORD Fusor 2001/2003 NG. Based on polyurethane, the product can be suitable for bonding composites parts in processes characterized by high production rates, such as in the automotive industry.

In comparison to conventional polyurethane adhesives, Fusor 2001/2003 NG reportedly maintains the same open time, but reduces from 2h30 to 45 min the handling time. “Due to the much faster cure curve, LORD Fusor 2001/2003 NG provides a considerable increase in productivity,” said Andrios de Souza, sales supervisor.

For more information, visit www.lord.com.