World’s First REACH-Compliant Curing Agent Dominates the News
Readers were most interested in news from Bitrez about a new curing agent last week.
October 22, 2018
Bitrez Ltd. recently announced it has reportedly launched the world’s first ketamine epoxy curing agents to combat the withdrawal of conventional grades prohibited in Europe under REACH regulations.
The ketamines are characterized by low viscosity and long pot-life allowing formulation of epoxy systems that offer good working time and relatively fast thin film cure rate.
Read more…