This company plans to market 2-hydroxyethyl methacrylate phosphate as an anti-corrosion agent and flame retardant under the brand name VISIOMER® HEMA-P 70M. Typical product applications for the monomer include adhesives and plastics, coatings, fibers, composite resins, and gel coats.
“VISIOMER HEMA-P 70M offers new options for customers with special requirements for flame-retardant and anti-corrosion properties,” said Martin Trocha, Ph.D., head of the application monomers product line. “This monomer adds a specialty methacrylate with particular functionalities to Evonik’s portfolio and underscores our role as a solution provider for innovative customers.”