Used at a low dry film thickness (DFT 0.5-7 µ), Michelman’s ProHere E 00017 reportedly exhibits excellent adhesion to a variety of metals, including cold-rolled, electroplated, and hot-dipped galvanized steel.

MICHELMAN: Waterborne Polymer Dispersions and Emulsions

Formulated for use in sealers for fasteners and window fittings, ProHere E 00017 provides lubricity and enhanced corrosion resistance on electroplated metal.

May 16, 2019

Michelman recently announced that it has introduced the newest addition to its line of ProHere® waterborne polymer dispersions and emulsions for use in metal coatings. Formulated for use in sealers for fasteners and window fittings, ProHere E 00017 provides lubricity and enhanced corrosion resistance on electroplated metal.

Used at a low dry film thickness (DFT 0.5-7 µ), ProHere E 00017 reportedly exhibits excellent adhesion to a variety of metals, including cold-rolled, electroplated, and hot-dipped galvanized steel. Easily stripped from plating racks with a hot alkali solution, it contributes to metal preservation through its water, solvent, and acid resistance.

Michelman reports that this new material performed well in several areas, including salt spray tests, consistent COF measurements, and gloss. It is suitable for plating applications in many segments, including automotive and construction applications.