IPS Adhesives Center of Excellence Leads the News
Last week, readers were most interested in IPS Adhesives’ announcement regarding its new manufacturing facility.
Last week, readers were most interested in IPS Adhesives’ announcement regarding its new manufacturing facility (IPS Adhesives Establishes Manufacturing Center of Excellence in North Carolina): “IPS Adhesives recently announced that it has established a manufacturing Center of Excellence in its Durham, N.C., ISO 9001:2015-certified facility. The new center coincides with recent investments in production, including those planned or already in progress, as well as the company’s efforts in centralizing its North American R&D and customer service activities at the facility.
“According to the company, the facility will provide customers with enhanced on-time delivery and faster response times through new, more agile processes. Part of this includes an established standard stocking of 165 of the company’s best-selling colors, with the ability to quickly produce another 100+ colors to order.
“Creating the Center of Excellence also reportedly included several changes following IPS’ Continuous Improvement process, which added more production cells and increased output. It also involved the implementation of a new QC tinting/testing lab dedicated to surfacing adhesives and hosting the latest color-matching and verification technology. With the upgrades, the company’s transition is complete for the manufacturing of surfacing adhesives under the Integra Adhesives brand from Abbotsford, Canada, to Durham. IPS reports that the shift will result in production and customer support teams being geographically closer to the majority of the market, thereby boosting service.”
Does your company have news to share with the industry? Please send your press releases to me at suttons@bnpmedia.com.
Top 5 News that Sticks for May 10-16
- IPS Adhesives Establishes Manufacturing Center of Excellence in North Carolina
- Henkel Collaboration Enables Remote Monitoring of COVID-19 Patients
third week in Top 5! - Mitsubishi Chemical Aims to Bolster its Technology Platform by Acquiring Gelest
- Avery Dennison Partners with Global Safety First to Produce Self-Adhesive N95 Masks for Healthcare Professionals
- Revenues Decline 5% for Huntsman in 2020 First Quarter
This weekly roundup highlights the adhesives, sealants, and coatings-related news stories that garnered the most attention during the previous week on our website, as well as our eNewsletters and social media platforms.