Vitralit UC 6685 is a transparent, UV-curing adhesive based on epoxy resin.
Vitralit® UC 6685 was reportedly formulated by Panacol specifically for decorations on plastic, glass, and metal. Due to its slight magnifying property, the transparent adhesive reportedly produces a high-quality image of the structures and illustrations underneath.
Vitralit UC 6685 is a transparent, UV-curing adhesive based on epoxy resin. Panacol reports that the viscosity of the one-component, easy-to-dispense adhesive makes it suitable for decorative applications on flacons and bottles or for dome coatings, an elegant protective coating for products such as key rings, lapel pins, buttons, name tags, pens, and jewelry.
Under UV light in the 320-390 nm wavelength range, Vitralit UC 6685 can reportedly be cured in just a few seconds, enabling a high cycle rate in the production process. After curing, Vitralit UC 6685 is very hard and scratch resistant. It is characterized by its brilliant transparency and does not yellow as it ages.
Additional details are available at www.panacol.com.