Avery Dennison EV adhesives
The EV battery portfolio includes single-coated, double-coated, and transfer tape constructions with a variety of liner options. (Photo courtesy of Avery Dennison Performance Tapes.)

AVERY DENNISON PERFORMANCE TAPES: Adhesive Solutions for Electric Vehicle Batteries

Applications include thermal runaway protection, cell-to-cell bonding, and compression pads.

May 20, 2021

Avery Dennison Performance Tapes has expanded its automotive offering with a portfolio of adhesive solutions for electric vehicle (EV) batteries. The EV battery portfolio offers bonding solutions coupled with functional properties such as flame retardancy and dielectric strength. These solutions can be used for a variety of applications, including thermal runaway protection, cell-to-cell bonding, and compression pads. The new portfolio enables EV battery and component manufacturers to tailor adhesives to the application while eliminating the cure times and equipment required with liquid adhesives.

"EV batteries are one of the fastest growing segments of the automotive industry, and component manufacturers need bonding solutions that meet their high-performance requirements while streamlining production," said Michael VanHaerents, automotive business development manager at Avery Dennison Performance Tapes. "We're pleased to build upon our experience serving the automotive industry and expertise engineering flame-retardant adhesives with the launch of this new portfolio."

The EV battery portfolio includes single-coated, double-coated, and transfer tape constructions with a variety of liner options. A range of adhesive chemistries (including acrylic, silicone, and rubber) allows manufacturers to match adhesion, shear, and environmental resistance to battery pack specifications.

Flame-retardant adhesives included in the portfolio are engineered to bond with and facilitate composites and materials to meet UL® 94 V-0 and other flame-retardant requirements. In addition to bonding, these single-coated and double-coated constructions feature conductive and nonconductive properties that provide manufacturers with new solutions for reducing vibration degradation of materials, reflecting radiant heat, and flame-energy mitigation.