Dow to Build MDI Distillation and Prepolymers Facility in Texas

In coordination with the startup of a new MDI facility in Freeport, Dow will shut down the polyurethane assets at its La Porte site.

June 14, 2021

Dow recently announced plans to build an integrated methylene diphenyl diisocyanate (MDI) distillation and prepolymers facility at its world-scale manufacturing site in Freeport, Texas. According to Dow, this investment supports increasing demand for downstream polyurethane systems products and advances the company’s positions in applications for construction, consumer, and industrial markets that are growing above GDP.

The new Freeport MDI facility will replace Dow’s current North America capacity in La Porte, Texas, and will also be capable of supplying an additional 30% of product to Dow’s customers. In coordination with the startup of the new MDI facility, expected in 2023, Dow will shut down its polyurethane assets at the La Porte site.

“This MDI investment optimizes our existing asset infrastructure and enhances our global polyurethanes leadership position, further enabling us to support downstream systems customers’ growth,” said Jane Palmieri, president of Dow’s Industrial Intermediates & Infrastructure operating segment. “The back integration at the Freeport site creates a cost competitive supply of key upstream polyurethane raw materials, ensures a reliable supply position to support our growth in downstream high-value polyurethane markets and delivers a more sustainable production process.”

The new facility in Freeport will reportedly reduce Dow’s carbon footprint and water usage by:

  • Eliminating the need for the generation of thermal power by utilizing existing thermal energy from the Freeport site
  • Reducing water intake and wastewater discharge (through production efficiencies)
  • Eliminating the need for transport of raw materials