www.adhesivesmag.com/articles/98887-henkel-dual-cure-optical-adhesive
Henkel optical adhesives
Dual-cure, active-alignment LOCTITE STYCAST OS 5101 reportedly provides dimensionally stable adhesion for optical lens and component bonding. (Image courtesy of Henkel.)

HENKEL: Dual-Cure Optical Adhesive

The adhesive allows precise positioning of optical lenses within a transceiver optical sub-assembly.

October 5, 2021

Henkel has developed LOCTITE® STYCAST® OS 5101, a dual-cure adhesive for optimal, precise optical lens and component alignment during the in-line assembly process for optical transceivers in next-generation cloud and hyperscale data centers. The new material reportedly builds on the company’s growing portfolio of data center optics products and has been designed to provide excellent alignment accuracy for maximum light transmission in high-speed optical transport network solutions.

“As cloud-scale and hyperscale data centers continue to evolve to meet demanding data management bandwidth expectations, data center interconnections are becoming increasingly more powerful and efficient,” said Wayne Eng, Henkel’s global head of Data & Telecom Market Strategy. “Transceivers are the key building blocks for high-speed data transmission and their assembly integrity is more critical than ever before to protect device investment, ensure long-term reliability, and optimize function.”

“Transceiver development has dramatically accelerated to keep pace with the exponential data processing demands, as is evidenced by the quick move from 100 GbE to 400 GbE to now 800 GbE modules,” said Tim Munks, senior principal analyst at Omdia. “Over the next four years, we expect the unit volume CAGR for 400 GbE to be greater than 200% and more than 300% for 800 GbE. Optical communication efficiency is the key to meeting the expectations for cloud, video, gaming, work and learn from home applications—and it is only getting more intense. Transceiver reliability, signal integrity and lower loss optics are critical.”

In order for optical signals to transmit with minimal loss, meticulous alignment of lenses and optical components is required. After a first-stage UV partial cure, LOCTITE STYCAST OS 5101 allows precise positioning of optical lenses within the transceiver optical sub-assembly. Once final thermal curing takes place, the material maintains its dimensional stability to ensure accurate lens position while in operation. In addition to high reliability as confirmed by high temperature/high humidity, thermal shock, and high temperature storage testing, internal results also indicate that material properties of LOCTITE STYCAST OS 5101 are capable of delivering other important performance metrics for 100GbE to 400GbE transceiver optical bonding, such as: maximized optical signal through positional integrity and dimensional stability; and high UPH capability with energy savings.

“The tight tolerance for lens and component movement leaves no room for error,” Eng said. “Achieving demanding dimensional stability and reliability standards required for next-generation optical components and transceivers is possible with LOCTITE STYCAST OS 5101.”