The Master Bond EP40TC two-part epoxy system for bonding, sealing, and encapsulating meets NASA low outgassing requirements and is able to transfer heat without conducting electricity. (Image courtesy of Master Bond.)
MASTER BOND: Thermally Conductive, Electrically Nonconductive, Low-Outgassing Epoxy
Master Bond EP40TC is a two-part epoxy system designed for bonding, sealing, and encapsulating applications where thermal conductivity and electrical insulation are required. With a high thermal conductivity value of 8-11 BTU•in/(ft2 •hr•°F) [1.16-1.60 W/(m•K)], it is formulated with a small particle size filler, making it ideal for filling small cavities and applying the product in thin sections. Its volume resistivity is greater than 1015 ohm-cm.
“EP40TC’s key distinguishing factor is that there is no compromise on the bond strength while providing excellent elongation and toughness,” said Rohit Ramnath, senior product engineer. “It has a high strength profile with a tensile lap shear strength of 2,300-2,500 psi, an elongation of 60-70%, and a tensile modulus of 5,000-15,000 psi. Also, it meets NASA low outgassing specifications which is a prerequisite for many aerospace, electronic, and optical applications.”
Reportedly serviceable from -100°F to +300°F, this toughened system resists thermal cycling, vibration, and shock. EP40TC exhibits a high peel strength of 40-60 pli and Shore D hardness of 70-80 at 75°F. It features a 1:1 mix ratio and cures in 2-3 days at room temperature (faster with the addition of heat). This compound adheres well to a variety of substrates, such as metals, composites, glass, and many plastics. EP40TC is available in standard packaging, as well as premixed and frozen syringes.
Additional details are available at www.masterbond.com.