Fluoramics reports that its premium full-density PTFE tape is waterproof, approved for oxygen service, and safe for use in cryogenics and with harsh chemicals. (Image courtesy of Fluoramics.)

FLUORAMICS: Oxygen-Safe Polytetrafluoroethylene (PTFE) Tape

June 30, 2022

Fluoramics has added additional sizes to its selection of LOX-8 full-density polytetrafluoroethylene (PTFE) tapes, now offering a 1/4-in. width and lengths of 260 and 520 in. According to the company, this width was previously difficult to find in the full-density, oxygen-safe formula.

Specifications of LOX-8 full-density PTFE tape include:

  • Temperature range of -400°F (-240°C) to 550°F (+287°C)
  • Use in cryogenic applications
  • Waterproof
  • MIL-T-27730A
  • A-A-58092
  • FDA approved for food use 21 CFR 177.1550