EPS 2121 is an all acrylic general-purpose pressure-sensitive adhesive emulsion for removable applications. EPS 2121 exhibits low peel, moderate tack and high shear values. Typical values below are for the neat polymer.
180 Peel (PSTC-101) 1.4 lbs/in.
Loop Tack (PSTC-16) 2.3 lbs/square in,