Converters Turn to Slot-Die Coaters to Increase Quality, Reduce Emissions
One reason for the increased attractiveness of slot-die coating is that the intense competition generated by industry consolidation and globalization has increased pressure to maximize economy, productivity and quality assurance. Quality is especially critical in medical, electronic, photographic and other high-end markets. At the same time, there is a growing mandate for further reductions in emissions of volatile organic compounds (VOCs) from solventborne coating systems.
The slot-coating die differs from the roll coater in two critical respects:
Exclusive Insights: Gain access to in-depth coverage of adhesive and sealant manufacturing, formulations and finished products. Comprehensive Coverage: Stay informed with the latest news and trends through our videos, podcasts, eNewsletters, webinars, continuing education resources, and a monthly eMagazine. Networking Opportunities: Connect with other industry professionals and leaders through our webinars and online platforms.