To meet the needs of member companies and others that will be affected by the Paper & Other Web Coating Maximum Achievable Control Technology Rule, the Pressure Sensitive Tape Council has developed the one-day EPA P&OWC MACT Rule Training Program seminar.
Chemir announces the acquisition of Guidelines Integrated Services, Miramar, FL, expanding Chemir's pharmaceutical contract research and development organization to now include three locations and approximately 100 employees.
Advanced Chemistry & Technology (AC TECH) announced that its new low density, fast cure fuselage sealant, AC-770 Class B2, is now fully qualified to Boeing Commercial Airplane Group's BMS 5-142 Type II, Class B2 specification.
Akzo Nobel will form a new unit, Ink & Adhesive Resins, by merging the businesses Printing Ink Resins and Pine Specialties, with a combined total of 550 employees.
The BroadBeam line of electron beam processors is available as a result of the acquisition of this technology by PCT Product & Manufacturing LLC from Bemis Clysar, Inc.