Scott Bader recently announced it has received the Composites UK 2013 Innovation in Materials industry award for its Crestabond® MMA structural adhesives range.
The partial shutdown of the federal government earlier this month reportedly didn’t take the steam out of the U.S. economy, according to the American Chemistry Council’s (ACC) monthly Chemical Activity Barometer (CAB).
Momentive Specialty Chemicals Inc. recently announced that it has signed a non-binding memorandum of understanding with Kanoria Chemicals & Industries Ltd. to form a joint venture.