Standards that will measure the properties of hydrocarbon resins are being developed by American Society for Testing and Materials (ASTM) Subcommittee D01.38 on Hydrocarbon Resins.
A corporate video profiling the Construction & Distribution Division of Bostik has been honored with a Bronze Telly Award in a highly respected national competition of film, video, cable and non-network television programming.
The National Paint and Coatings Association (NPCA) and a group of aerosol adhesives manufacturers have proposed to the California Air Resources Board (CARB) an industry-drafted standard for regulating volatile organic compounds (VOCs) from aerosol adhesives.