Covestro exhibited its portfolio of sustainable coating solutions at the recent 2022 American Coatings Show, helping pave the way for a shift to the circular economy.
Michelman is showcasing its waterborne coating additives with a focus on high-performance wood applications as well as bio-based and renewable products at the American Coatings Show (ACS) 2022.
Arkema recently announced that it is showcasing a broad offering of coating materials for waterborne, high solids, UV/EB, and powder formulations at the 2022 American Coatings Show (ACS) in Indianapolis, Ind., April 5-7, booth #1130.
Chromaflo Technologies will be exhibiting at the American Coatings Show, set to take place at the Indiana Convention Center in Indianapolis, Ind., from April 5-7.
Builder confidence in the market for newly built single-family homes moved two points lower to 79 in March from a downwardly revised reading in February, according to a recent National Association of Home Builders (NAHB)/Wells Fargo Housing Market Index (HMI).
A newly synthesized PCD-PPG block copolyether polyol can be applied to coating applications that require flexibility, in solvent-free urethane compositions that require low viscosity, and in various other CASE applications.
A new polyol (PCD-b-PPG) has been synthesized that has a low viscosity of around 800-3,000 mPa·s (at 25˚C, liquid state) and is transparent due to the use of PCD as an initiator, even after storing for a long duration. The new PCD-b-PPG polyol can be applied to coating applications where transparency is required. In addition, it may contribute to other CASE applications and solvent-free urethane compositions that can take advantage of its low viscosity.
Indianapolis will welcome coatings industry professionals from around the world for the 2022 American Coatings Show.
March 16, 2022
The American Coatings Show and Conference returns to the Indiana Convention Center in Indianapolis, Ind., on April 5-7, 2022. Through the event’s conference and exhibition, coatings industry professionals will have myriad opportunities to learn about the latest technologies in raw materials for coatings and adhesives, processing and testing equipment, and environmental protection and safety, as well as a range of services.