What are some fundamental issues that I should know regarding the basics of formulating coatings?
May 1, 2015
An important concept to learn is critical pigment volume concentration (CPVC). Understanding this concept is essential for formulating high-performance coatings. In fact, it’s an “elephant in the room” for many formulators—ignored at our peril.