This company has introduced its new line of ARclean™ acrylic acid and organotin-free, strippable, electronically clean, pressure sensitive adhesive products.
This company’s new product, 118-09, is a two-component, solvent-resistant, electrically conductive ink, coating and adhesive suitable for screen-printing printed circuit lines.
Mereco Metrethane™ 4716 is a new, two-component, low-viscosity polyurethane gel that has been specifically designed for cable sealing, potting cable connectors and telecommunications repairs where excellent resistance to salt water and fuel oils is needed.