Henkel reports that Teroson EP 5020 TR can be applied at room temperature in a smooth, flameless, and solder-free process.
April 7, 2020
Henkel recently introduced Teroson EP 5020 TR, a two-component epoxy-based cold rebuilding material designed to replace conventional tin solder in aftermarket repairs of automotive body damages.
According to Toyochem, TSS510-HF addresses the needs of today’s electronics designers for improved shielding performance for the transmission of high-frequency signals and for high flexibility so circuits do not break when bent.
April 2, 2020
Toyochem Co., Ltd., a member of the Toyo Ink Group, has launched a flexible electromagnetic interference (EMI) shielding film, LIOELM TSS510-HF, designed to meet the performance requirements of 5G flexible printed circuits (FPCs).
EP21TPHT is an electrically insulating material with a dielectric constant of 3.9 and volume resistivity of more than 1,014 ohm-cm at 75˚F.
March 26, 2020
Master Bond EP21TPHT is a new two-component epoxy polysulfide system designed for bonding applications that require toughened and thermally stable bonds that are resistant to chemicals.
Due to its high viscosity, Vitralit UC 1536 is particularly suitable for applications that require dimensional stability within the production process.
March 24, 2020
Panacol recently announced that it has launched Vitralit UC 1536, a low-halogen UV adhesive for the electronics industry.
This thermally conductive compound reportedly offers high dielectric properties with a volume resistivity of 1,015 ohm-cm.
March 19, 2020
EpoxySet recently announced that it supplies EC-1012M/EH-20 flame-resistant potting compound for protecting power supplies, high-voltage batteries, coil windings, transformers, PC boards, and other electronic devices.
Formula-8 is reportedly a shear-sensitive paste that sheets out into polytetrafluoroethylene (PTFE) strings when torqued and delivers high sealing performance on all sizes of threads.
March 17, 2020
Fluoramics, Inc. recently introduced a new application tip for its 100-g tube of Formula-8 thread sealant.
Recommended applications for SikaLastomer-714 include the sealing of bolt-in parts to vehicle flanges (i.e., truck sliders), as well as the sealing of gaskets to various substrate materials.
March 12, 2020
Sika Corp. recently introduced its SikaLastomer-714 butyl sealant for the U.S. transportation aftermarket.
Dispense Works reports that all motion, vision, and control system software for this dispensing system is written in house.
March 10, 2020
Dispense Works Inc. recently announced that its RP series robotic dispensing system with an optional vision-guided component performs pattern recognition and edge/hole detection for simpler setup and fixturing while assuring repeatability.
According to CVC, coverings and coatings made with its HyPox CTBN-modified epoxy resins can help protect pipelines from corrosion.
March 5, 2020
CVC Thermoset Specialties recently announced that it has developed advanced materials to help oil and gas pipeline engineers meet challenges such as corrosion, cathodic disbondment, and high-temperature resistance.